您的位置: 专家智库 > >

田轲

作品数:2 被引量:1H指数:1
供职机构:西南交通大学材料科学与工程学院材料先进技术教育部重点实验室更多>>
发文基金:国家高技术研究发展计划更多>>
相关领域:理学一般工业技术更多>>

文献类型

  • 2篇中文期刊文章

领域

  • 1篇一般工业技术
  • 1篇理学

主题

  • 2篇T-ZNOW
  • 1篇微观形貌
  • 1篇光催化
  • 1篇光催化性
  • 1篇光催化性能
  • 1篇PHOTOC...
  • 1篇SIMPLE
  • 1篇ZNO
  • 1篇HETERO...
  • 1篇催化
  • 1篇催化性
  • 1篇W
  • 1篇CDS
  • 1篇NANOPA...
  • 1篇HETERO...

机构

  • 2篇西南交通大学

作者

  • 2篇范希梅
  • 2篇田轲
  • 1篇代佳
  • 1篇周祚万
  • 1篇张冯章
  • 1篇吴德智
  • 1篇刘花蓉
  • 1篇吴德志

传媒

  • 1篇材料导报
  • 1篇Transa...

年份

  • 2篇2012
2 条 记 录,以下是 1-2
排序方式:
Fabrication and photocatalytic properties of Cu_2S/T-ZnO_w heterostructures via simple polyol process被引量:1
2012年
The Cu2S/tetrapod-like ZnO whisker(T-ZnOw) heterostructures were successfully synthesized via a simple polyol process employing the poly(vinyl pyrrolidone)(PVP) as a surfactant.The as-prepared heterostructures were characterized by X-ray diffraction(XRD),field emission scanning electron microscopy(FESEM),X-ray photoelectron spectroscopy(XPS) and Fourier transform infrared(FTIR).The photocatalytic properties of Cu2S/T-ZnOw nanocomposites synthesized with different PVP concentrations were evaluated by photodegradation of methyl orange(MO) under UV irradiation.The results show that the Cu2S/T-ZnOw nanocomposites exhibit remarkable improved photocatalytic property compared with the pure T-ZnOw.The sample prepared with 3.0 g/L PVP shows an excellent photocatalytic property and the highest photodegradation rate of MO is 97% after UV irradiation for 120 min.Besides,the photocatalytic activity of the photocatalyst has no evident decrease even after four cycles,which demonstrates that the Cu2S/T-ZnOw photocatalyst exhibits an excellent photostability.Moreover,the photocatalytic mechanism of the Cu2S/T-ZnOw nanocomposites was also discussed.
吴德智范希梅田轲代佳刘花蓉
CdS/T-ZnO_w复合材料的制备及光催化性能研究
2012年
采用化学水浴沉积法在T-ZnOw表面上沉积CdS纳米颗粒,用X射线衍射仪、扫描电镜和场发射表征样品的结构和形貌。并且在常温(25℃)下测试了CdS/T-ZnOw复合材料的光催化性能。结果表明,CdS/T-ZnOw复合材料的光催化性能直接受NH4Cl浓度的影响,可通过调控NH4Cl的浓度来调控CdS纳米颗粒的微观形貌。在0.74~2.99mmol/L范围内,CdS/T-ZnOw复合材料的光催化性能随NH4Cl浓度的增大而增大,在2.99~7.4mmol/L范围内,光催化性能随NH4Cl浓度的增大而减小。
田轲范希梅张冯章吴德志周祚万
关键词:T-ZNOWCDS微观形貌光催化性能